Description
Two-component epoxy primer MONE 801 consists of: component A (epoxy resin) and component B (hardener). Used for priming concrete, aerated concrete, brick and metal structures. Provides adhesion, removes dust from the substrate, with the possibility of further application of polyurea coatings.
Characteristics
Physical and chemical properties
|
Property |
Units | Value | |
| Component A (Resin) | Component B (Hardener) | ||
| 1. Appearance | Visual | Homogeneous transparent viscous liquid | Homogeneous yellow-brown liquid |
| 2. Viscosity (Brookfield, spindle 3, 25 oC), max | Pa∙s | 15 | 4 |
| 3. Density (25oC) | g/m3 | 1.40 | 0.9 - 1.1 |
| 4. Solids content | % | 96 | |
| 5. Pot life of the mixture (20oC) | min | 30-45 | |
Mix ratio by weight: Component A : Component B = 100:25
Technological properties
| Property | Value | Test method |
| Bending elasticity, mm | 1 | GOST 52740-2007 |
| Impact strength, cm | 50 | GOST R 53007-2008 |
| Hardness, Shore D | 75-80 | DIN 53505 (after 7 days at +23°C) |
| Adhesion, MPa, min | 2.5 | GOST 32299-2013 |
| Tack-free time, h (25°C) | 3-5 | GOST 19007-73 |
| Curing time of thin layers, h (25°C) | 9-10 | GOST 19007-73 |
Application technology
For professional use only!
To obtain a quality coating, surface preparation must be carried out in accordance with applicable construction and technical standards (the surface must be dry, degreased, and free of dirt, dust and old coating).
Do not mix the components by hand!
- Recommended substrate temperature: from +15 to +25°C.
- Recommended air temperature: from +15 to +25°C.
- Recommended substrate moisture: no more than 4%.
- Recommended thickness of one layer: 50÷70 μm.
Recommended number of layers as a primer coat:
- For non-porous materials: 1÷2,
- For porous materials: 2÷3.
Recommended recoat interval at +20°C is from 8 to 24 hours; exceeding the recoat interval reduces adhesion. If there are no signs of gelling or thickening of the mixture, it may still be used.
The substrate temperature during application and until the coating is fully cured must be at least 3°C above the dew point. Condensation forming on the concrete surface during application and curing of the polymer coating may cause defects and lead to partial or complete delamination from the concrete substrate. Drafts during application may also cause coating defects such as orange peel or rippling.
Equivalents
Sikafloor-150; Sikafloor-151; Sika Primer-150 MB; Sipp-Epoxy Primer HS; LEVL Coat 101; LEVL Coat 102W
Related products

Epoxy Self-Levelling Floor MONE 820
Two-component epoxy self-levelling floor MONE 820
Details →
Polyurethane self-levelling floor MONE 720
Polyurethane self-levelling floor MONE 720 is a two-component, coloured polyurethane compound for creating polymer coatings.
Details →
Transparent Epoxy Self-Levelling Floor MONE 823D
Epoxy compound for 3D floor installation MONE 823D
Details →
MONE Polycem 3K AS polyurethane-cement system
Polyurethane-cement system for medium and heavy-duty service conditions "MONE Polycem 3K AS".
Details →Need a quote or technical advice?
Tell us about your application, volumes and destination. Our team will reply with a proposal and technical data sheets.